PRESTRESSED CONCRETE PILES
I  Shape piles
Section  :  I   Type  :  I-0.15 x 0.15 x 12.0 M.
Concrete
>>
High early strength Portland cement type III is used in order to meet the American Standard
(ASTM Designation C150) and ingredient of concrete is not less than 400 kg/m3
   
>>
The ultimate compressive strength is not less than 450 kg/ sq cm. by experiment with the concrete cubic at
15 x 15 x 15 cm or not less than 350 kg/ sq cm, tested with cylinder concrete. Radial 6” x 12” at 28 days age.
   
>>
The compressive strength will be transferred into concrete texture, when the compressive strength of concrete
  is not less than 245 kg/ sq cm.
   
>>
Pre – Tensioning Method is applied in our process.
   
>>
Concrete curing with water.
   
Uncoated Stress - Relieved Wires (High tension wires)
>>
Uncoated Stress-Relieved Steel Wire Indented Round Type for Single wire. Diameter size is   4 mm, 5 mm.
   
>>
Ultimate Compressive Stress is not less than 17,500 kg/sq.cm.
   
>>
High tension wires of tensile strength are not less than 70-75%.
   
Stirrups
>>
Used Structural Grade, diameter size is 3.0 mm, 4.0 mm and 6.0 mm.
   
>>
Have elastic strength is not less than 2,400 kg / sq.cm.<
   
>>
The ultimate compressive strength is not less than 450 kg/ sq cm.
   